Products

  • SUPER DUPLEX S32760 / F55 / 1.4501

    Super Duplex S32760/ F55 , Super Duplex Alloy UNS S32760 (F55 / 1.4501) has excellent resistance Pitting and Crevice Corrosion in seawater at elevated temperatures, supplied with a PREN 40<( Pitting Resistance Eqv) . Excellent resistance to SCC ( Stress Corrosion Cracking) in Sour and Chloride environments .

  • 17-7 Steel Strip, Coil, Foil, Wire, AMS 5528 (CONDA), AMS 5529 (COND C), ASTM A693, MIL-S25043

    ● Springs
    ● Washers
    ● Clips
    ●Surgical parts
    ● Blades
    ● Bellows
    ● Honeycomb

  • Hastelloy B

    Hastelloy B is a solid solution strengthened, nickel-molybdenum alloy, with significant resistance to reducing environments like hydrogen chloride gas, and sulfuric, acetic and phosphoric acids. Molybdenum is the primary alloying element which provides significant corrosion resistance to reducing environments. This nickel steel alloy can be used in the as-welded condition because it resists the formation of grain-boundary carbide precipitates in the weld heat-affected zone.

    This nickel alloy provides excellent resistance to hydrochloric acid at all concentrations and temperatures. In additions, Hastelloy B2 has excellent resistance to pitting, stress corrosion cracking and to knife-line and heat-affected zone attack. Alloy B provides resistance to pure sulfuric acid and a number of non-oxidizing acids.

  • 17-4PH Material Data Sheet

    International identifiers

    AISI 630, ASTM A564-89 17-4PH, JIS SCS24 / SUS630, AFNOR Z7CNU15-05 / Z7CNU17-04

  • Stainless Steel 904L 1.4539

    This data sheet applies to stainless steel 904L / 1.4539 hot and cold rolled sheet and strip, semi-finished products, bars, rolled wire and profiles as well as seamless and welded tubes for pressure purposes.

  • IInconel

    High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Fe Al Ti Cu Mo Nb other no greater than Inconel600 0.15 0.5 1 0.015 0.03 14~17 base 6~10 - - ≤0.5 - - - Inconel601 0.1 0.5 1 0.015 0.03 21~25 base 10~15 1~1.7 - ≤1 - - - Inconel625 0.1 0.5 0.5 0.015 0.015 20~23 base ≤5 ≤0.4 ≤0.4 - 8~10 3.15~4.15 Co≤1 Inconel725 0.03 0.2 0.35 0...
  • Shaped, Flat, Square, Round, Fine, Plated and Bare Wire ASTM A167, AMS 5523

    Alloy 310S is an austenitic chromium nickel stainless steel that posses good oxidation resistance and strength at high temperatures in continuous service up to 2000ºF (provided reducing sulfur gasses are not present). It is also used for intermittent service at temperatures up to 1900°F because it resists rescaling and has a low coefficient of expansion. This factor reduces the tendency of the steel to warp in heat service. Alloy 310S is similar to alloy 310 except for lower carbon content to minimize carbide precipitation during welding.

  • Alloy

    High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Fe Al Ti Cu Mo Nb other no greater than Inconel600 0.15 0.5 1 0.015 0.03 14~17 base 6~10 - - ≤0.5 - - - Inconel601 0.1 0.5 1 0.015 0.03 21~25 base 10~15 1~1.7 - ≤1 - - - Inconel625 0.1 0.5 0.5 0.015 0.015 20~23 base ≤5 ≤0.4 ≤0.4 - 8~10 3.15~4.15 Co≤1 Inconel725 0.03 0.2 0.35 0...
  • ALLOY 625 MATERIAL DATA SHEETS

    Alloy 625 is a nonmagnetic , corrosion – and oxidation-resistant, nickel-based alloy. Its outstanding strength and toughness in the temperature range cryogenic to 2000°F (1093°C) are derived primarily from the solid solution effects of the refractory metals, columbium and molybdenum, in a nickel-chromium matrix. The alloy has excellent fatigue strength and stress-corrosion cracking resistance to chloride ions. Some typical applications for alloy 625 have included heat shields, furnace hardware, gas turbine engine ducting, combustion liners and spray bars, chemical plant hardware, and special seawater applications.

  • HASTELLOY B2 UNS N10665 W.NR.2.4617

    Hastelloy B2 is a solid solution strengthened, nickel-molybdenum alloy, with significant resistance to reducing environments like hydrogen chloride gas, and sulfuric, acetic and phosphoric acids. Molybdenum is the primary alloying element which provides significant corrosion resistance to reducing environments. This nickel steel alloy can be used in the as-welded condition because it resists the formation of grain-boundary carbide precipitates in the weld heat-affected zone.

    This nickel alloy provides excellent resistance to hydrochloric acid at all concentrations and temperatures. In additions, Hastelloy B2 has excellent resistance to pitting, stress corrosion cracking and to knife-line and heat-affected zone attack. Alloy B2 provides resistance to pure sulfuric acid and a number of non-oxidizing acids.

  • Hastelloy

    High Temperature Alloy Chemical composition Grade C P S Mn Si Ni Cr Co Cu Fe N Mo Al W V Ti other no greater than HastelloyB 0.05 0.04 0.03 1 1 base ≤1 ≤2.5 - 4~6 - 26~30 - - 0.2~0.4 - - HastelloyB-2 0.02 0.04 0.03 1 0.1 base ≤1 ≤1 - ≤2 - 26~30 - - - - HastelloyB-3 0.01 0.04 0.03 3 0.1 ≥65 1~3 ≤3 ≤0.2 1~3 - 27~32 ≤0.5 ≤3 ≤0.2 ≤0.2 - ...
  • Hastelloy C-276 MATERIAL DATA SHEETS

    HASTELLOY C276, UNS N10276 is considered the most versatile corrosion resistant nickel alloy available. Alloy C-276 also has excellent resistance to pitting, stress-corrosion cracking, especially suitable for use in high temperature, inorganic and organic acids mixed with impurities (such as formic acid and acetic acid), and seawater corrosive environments.

123 Next > >> Page 1 / 3